шарового измельчения (bwi) и индексом падающего груза dwi. 123 шего объема информац...The grindability of an ore in the process of mineral dressing can be determined by use of the Bond work index (Wi). This index is determined on a laboratory-scale using a Bond ball-mill and by ...